Poly(3,4-ethylenedioxythiophene)-poly(styrenesulfonate)
Catalog Number
ACMA00000154
Synonyms
Poly(2,3-dihydrothieno-1,4-dioxin)-poly(styrenesulfonate), Orgacon ICP 1050, PEDOT:PSS
Description | 1.1% in H2O, surfactant-free, high-conductivity grade |
IUPAC Name | 2,3-dihydrothieno[3,4-b][1,4]dioxine;(E)-2-phenylethenesulfonic acid |
Molecular Weight | 326.4g/mol |
Molecular Formula | C14H14O5S2 |
Canonical SMILES | C1COC2=CSC=C2O1.C1=CC=C(C=C1)C=CS(=O)(=O)O |
InChI | InChI=1S/C8H8O3S.C6H6O2S/c9-12(10,11)7-6-8-4-2-1-3-5-8;1-2-8-6-4-9-3-5(6)7-1/h1-7H,(H,9,10,11);3-4H,1-2H2/b7-6+; |
InChI Key | BGAWZPQKJPTIEA-UHDJGPCESA-N |
Flash Point | Not applicable |
Purity | 1.3 wt % dispersion in H2O, conductive grade |
Density | 0.999 g/mL at 25 °C |
Application | PEDOT:PSS can be used as an electrode material with high mobility for charge carriers. It can be used for a wide range of energy based applications such as organic photovoltaics (OPV), perovskite solar cells (DSSCs), organic light emitting diodes (OLEDs) and other biomedical sensors.Used to prepare highly transparent conductive coating formulations. Primary and secondary nucleation by introducing PEDOT:PSS in a hydrogel was studied.Virtually 100% absorption from 900-2,000 nm. No absorption maximum from 400-800 nm. Conductive polymer blend. |
Storage | 2-8°C |
Composition | PEDOT content, 0.5 wt. % |
Concentration | 1.3 wt % dispersion in H₂O |
Conductivity | 1 S/cm |
Dimension | <200 nm, coeff var >95% |
Grade | conductive grade |
Impurity Content | <300 ppm Na |
MDL Number | MFCD07371079 |
Packaging | 100 g |
pH | 1.2-1.8 |
Quality Level | 100 |
Viscosity | <20 cP(20 °C) |