Description | ICBA is a C60 derivative that can be synthesized from C60 and indene. It is an acceptor material with shallow lowest occupied molecular orbital(LUMO) which can be used to enhance the performance of polymeric solar cells(PSCs). |
---|---|
Molecular Weight | 952.99 |
Molecular Formula | C78H16 |
Canonical SMILES | C1C2C3=CC=CC=C3C1C45C26C7=C8C9=C1C2=C3C%10=C9C9=C%11C%12=C%10C%10=C%13C%14=C%12C%12=C%15C%16=C(C4=C4C%17=C%16C%16=C%18C%19=C%17C%17=C%20C%21=C%19C%19=C%22C%23=C%21C%21=C(C1=C7C(=C%21%20)C6=C%174)C2=C%23C(=C3%10)C%221C%13(C2CC1C1=CC=CC=C21)C(=C%18%19)C%14=C%15%16)C(=C%12%11)C5=C98 |
InChI | InChI=1S/C78H16/c1-2-6-12-11(5-1)15-9-16(12)76-69-53-37-23-25-41-29(37)30-38-24-26-42(30)58-57(41)73-65-49(25)33-31-43-19-21-39-27-28-36-20-22-40(28)56-55(39)71(63(65)47(21)33)77-17-10-18(14-8-4-3-7-13(14)17)78(73,77)74(58)66-50(26)34(48(22)64(66)72(56)77)32-44(20)60(62(46(24)32)70(76)54(38)53)68-52(36)51(35(19)27)67(75(15,68)76)59(43)61(69)45(23)31/h1-8,15-18H,9-10H2 |
InChI Key | YLXQIZGBVUNXAF-UHFFFAOYSA-N |
Melting Point | 260 °C |
Purity | >98.5%HPLC |
Appearance | Black powder to crystal |
Application | ICBA can be used with poly(3-hexylthiophene)(P3HT) as an active layer which can be used in the fabrication of organic solar cells(OSCs).ICBA in combination with thiazolo-thiazolo can be used as a donor. It can be blended with PCBM for photovoltaic based application. |
Storage | Store under inert gas |
Assay | 99% (HPLC) |
Form | ITO/PEDOT:PSS/P3HT: ICBA (1:1)/Al• Short-circuit current density (Jsc): 10.82 mA/cm2 • Open-circuit voltage (Voc): 0.78 V• Fill Factor (FF): 0.56• Power Conversion Efficiency (PCE): 4.65 % |
MDL Number | MFCD20264904 |
OPV Device Performance | ITO/PEDOT:PSS/P3HT: ICBA (1:1)/Al • Short-circuit current density (Jsc): 10.82 mA/cm2 • Open-circuit voltage (Voc): 0.78 V • Fill Factor (FF): 0.56 • Power Conversion Efficiency (PCE): 4.65 % |
Orbital Energy | LUMO 3.67 eV (CV) |
Packaging | 250 mg in glass insert |
Quality Level | 100 |