| Description | Graphene preparation method: Electrochemical exfoliation. • Graphene thickness by AFM: 80%, 1-3 layers. • Sheet size by AFM: 10 μm. • Oxygen content: 7.5% (by XPS) (C/O-ratio: 12.3). • Raman I_D/I_G ratio: 0.4. • Sheet resistance: 4.8 kΩ/sq. • Typical properties of films produced thereof (after spray coating): a) 11 nm film: 90% transmittance, 1200 Ω/sq (as made). b) 20 nm film: 80% transmittance, 500 Ω/sq (as made). | 
|---|---|
| Appearance | dispersion (in DMF) | 
| Application | An excellent material for studying electrochemistry. | 
| Storage | room temp | 
| Concentration | 0.2 mg/mL (PEDOT:PSS) | 
| Form | dispersion (in DMF) | 
| Packaging | 50 mL in glass bottle | 
| Quality Level | 100 |